Microstructural analysis of thermal fatigue damage in 316L pipes

Gonzalez Sanchez, Sergio, Ruiz, Ana and Nilsson, Karl-Fredrik (2013) Microstructural analysis of thermal fatigue damage in 316L pipes. Technical Report. European Union, Luxembourg.

[img]
Preview
Text
ldna26445enn.pdf - Published Version

Download (3MB) | Preview

Abstract

This report summarizes the data and main conclusions derived from microstructural characterisation of 316L pipes subjected to thermal fatigue with a peak temperature of 550°C. TOFD measurements are compared with measured crack depths from cut segments, and fracture mode and corrosion have been assessed by SEM and EDX, respectively.

Item Type: Report (Technical Report)
Subjects: F200 Materials Science
Department: Faculties > Engineering and Environment > Mechanical and Construction Engineering
Depositing User: Becky Skoyles
Date Deposited: 11 Nov 2015 09:46
Last Modified: 18 Mar 2016 12:01
URI: http://nrl.northumbria.ac.uk/id/eprint/24429

Actions (login required)

View Item View Item

Downloads

Downloads per month over past year

View more statistics